Processed FOAM Slitting Foam

Processed FOAM Slitting Foam

We can help you to solve slitting offerings with the help of our sophisticated equipment and experienced specialists. In any case, we specialize in shut tolerance slitting and will meet your requirements at each program. Don’t hesitate to contact with MEISHUO for your customized products and slitting needs.

Tabla de propiedades físicas (TDS):

Producto Espuma de polietileno reticulado
Times 5B 10B 15B 20B 25B 30B
PROPIEDADES FÍSICAS MÉTODO DE PRUEBA UNIDADES MÉTRICAS /
Densidad - Nominal ISO 845:2006 GB/T 6343-2009 kg/m³ 200±30 100±10 66±8 50±6 40±5 33±5
Dureza Shore Orilla C LX-C ° ≥65 55±5 45±5 35±5 30±5 25±5
Límite de tamaño Espesor Interno mm 3~6 3~8 3~8 3~10 3~12 3~15
Anchura ≤1200 ≤1600 ≤1800 ≤1800 ≤1800 ≤1800
Resistencia a la tracción TD ISO 1798:2008 GB/T 6344-2008 MPa ≥1300 ≥700 ≥400 ≥300 ≥250 ≥200
MD ≥1500 ≥800 ≥500 ≥400 ≥300 ≥200
Alargamiento a la rotura TD ISO 1798:2008 GB/T 6344-2008 % ≥140 ≥130 ≥120 ≥110 ≥100 ≥90
MD ≥140 ≥130 ≥120 ≥110 ≥100 ≥90
Resistencia al desgarro TD QB/T 1130-91 KN/m ≥8 ≥5 ≥3 ≥2 ≥1.5 ≥1.2
MD ≥8 ≥5 ≥3 ≥2 ≥1.5 ≥1.2
Dimensión Estabilidad (80℃,24h) TD ISO 2796:1986 GB/T 8811-2008 % ≤±1.0 ≤±1.0 ≤±1.5 ≤±2.0 ≤±3.0 ≤±3.0
MD ≤±1.5 ≤±2.0 ≤±3.0 ≤±3.5 ≤±4.0 ≤±5.0
Absorción de agua en condiciones 50% RH ISO 62:2008 GB/T 1034-2008 % ≤0.2 ≤0.2 ≤0.2 ≤0.3 ≤0.3 ≤0.3
Conductividad térmica ISO 8302:1991 GB/T 10294-2008 W/(m.k) ≤0.045 ≤0.045 ≤0.045 ≤0.04 ≤0.04 ≤0.04

Escenarios de aplicación y requisitos de rendimiento:

Indicadores de resultados: High-temperature resistance, flame retardancy, rebound resilience

Indicadores de resultados: Thermal insulation, water resistance, aging resistance

Indicadores de resultados: Environmental non-toxicity, tear resistance, rebound resilience