Processed FOAM Slitting Foam

Processed FOAM Slitting Foam

We can help you to solve slitting offerings with the help of our sophisticated equipment and experienced specialists. In any case, we specialize in shut tolerance slitting and will meet your requirements at each program. Don’t hesitate to contact with MEISHUO for your customized products and slitting needs.

Physical Property Table (TDS):

Product Crosslinked polyethylene foam
Times 5B 10B 15B 20B 25B 30B
PHYSICAL PROPERTIES TEST METHOD METRIC UNITS /
Density - Nominal ISO 845:2006 GB/T 6343-2009 kg/m³ 200±30 100±10 66±8 50±6 40±5 33±5
Shore Hardness Shore C LX-C ° ≥65 55±5 45±5 35±5 30±5 25±5
Size limit Thickness Internal mm 3~6 3~8 3~8 3~10 3~12 3~15
Width ≤1200 ≤1600 ≤1800 ≤1800 ≤1800 ≤1800
Tensile Strength TD ISO 1798:2008 GB/T 6344-2008 MPa ≥1300 ≥700 ≥400 ≥300 ≥250 ≥200
MD ≥1500 ≥800 ≥500 ≥400 ≥300 ≥200
Elongation at Break TD ISO 1798:2008 GB/T 6344-2008 % ≥140 ≥130 ≥120 ≥110 ≥100 ≥90
MD ≥140 ≥130 ≥120 ≥110 ≥100 ≥90
Tear strength TD QB/T 1130-91 KN/m ≥8 ≥5 ≥3 ≥2 ≥1.5 ≥1.2
MD ≥8 ≥5 ≥3 ≥2 ≥1.5 ≥1.2
Dimension Stability (80℃,24h) TD ISO 2796:1986 GB/T 8811-2008 % ≤±1.0 ≤±1.0 ≤±1.5 ≤±2.0 ≤±3.0 ≤±3.0
MD ≤±1.5 ≤±2.0 ≤±3.0 ≤±3.5 ≤±4.0 ≤±5.0
Water Absorption under 50% RH condition ISO 62:2008 GB/T 1034-2008 % ≤0.2 ≤0.2 ≤0.2 ≤0.3 ≤0.3 ≤0.3
Thermal Conductivity ISO 8302:1991 GB/T 10294-2008 W/(m.k) ≤0.045 ≤0.045 ≤0.045 ≤0.04 ≤0.04 ≤0.04

Application Scenarios and Performance Requirements:

Performance Indicators: High-temperature resistance, flame retardancy, rebound resilience

Performance Indicators: Thermal insulation, water resistance, aging resistance

Performance Indicators: Environmental non-toxicity, tear resistance, rebound resilience